464. Raised manhole frames, cover plates and joint bolts.─ Requirements of regulation 138shall apply.
In short
Raised manhole frames, cover plates and joint bolts for boilers under this chapter must meet regulation 138, which sets their thicknesses, pressure limits and bolting.
Written by IBRsource editors · last edited 2026-11-20. Explanations simplify and are not a design method, testing procedure or authorisation. Requirements come from the complete regulations, the Gazette and approved documentation.
Comparison pending: the IBR 1950 text in force on 30 September 2026 is not yet established for this provision, so no change is claimed (how this works).
Orientation hints (unverified)
These candidates come from automated heading matching against DPIIT's scanned historical print edition of IBR 1950. That edition uses imperial units and riveted-construction provisions, so it is not the operative 2026 predecessor text. Regulation numbers alone never prove equivalence.
| Historical 1950-edition reg. | Heading as OCR'd | Heading similarity | Source image |
|---|---|---|---|
| 33 | Plates | 100% | Chapter II (DPIIT scan), image 3 |
| 167 | Raised Manhole Frames and Cover Plates | 100% | Chapter III (DPIIT scan), image 11 |
| 572 | Raised manhole frames, cover plates and joint bolts | 100% | Chapter XII (DPIIT scan), image 5 |
IBR 1950 regulation 33 as last published in the DPIIT web edition (archived 2022)
Unofficial archived copy, not verified; see the regulation 33 page for its amendments.
| Reg. 33 MATERIALS OF CONSTRUCTION COPPER PLATES, STAY AND RIVET BARS |
| (a) Process.- The copper shall be fire-refined or electrolytic and hot-rolled from suitable cakes. (b) Chemical Composition.- The chemical composition of the plates shall be as follows:-
(c) Freedom from defects.- The plates shall be clean, smooth and free from defects and shall have a workmanlike finish. They shall be thoroughly annealed. (d) Rolling Margin.- No plate shall be under the specified thickness at any part, not more than 5% over the calculated weight. The scrap margin, partly sheared and left attached, shall be not less than 3 inches at the ends and 1½ inches at each side. (e) Tensile Tests.- One tensile test shall be taken from each plate as rolled. The tensile breaking strength, from Standard Test Piece A, shall not be less than 14 tons per sq. inch with an elongation of not less than 35%. (f) Hot and Cold Bend tests.- One hot (temperature between 1200°F and 1400°F) and one cold bend test shall be taken from each plate as rolled. For either hot or cold bend tests, the test piece shall withstand being doubled over without fracture until the sides are touching and parallel. |
IBR 1950 regulation 167 as last published in the DPIIT web edition (archived 2022)
Unofficial archived copy, not verified; see the regulation 167 page for its amendments.
| Reg. 167 MANHOLES, MUDHOLES, ETC. Raised Manhole Frames and Cover Plates
Welds should be positioned so that they are located on the transverse centre line of the boiler. The jointing flanges of mouthpieces and covers shall be machined on the face and edge and on the bearing surface for the bolts. Bolts and nuts shall be machined where in contact with the flanges and the joints should be formed inside and outside the bolts to preclude the possibility of flange distortion. Cover plates shall be dished outwards to a depth of approximately one-eighth of the internal diameter of the frame. All frames and mouthpieces shall bed closely to the surfaces to which they are to be connected, and where riveted to cylindrical shells shall be at least double riveted. All caulking edges shall be machined or machine gas cut. |
IBR 1950 regulation 572 as last published in the DPIIT web edition (archived 2022)
Unofficial archived copy, not verified; see the regulation 572 page for its amendments.
| Reg. 572, Reg. 573, Reg. 574 | |||||||||||||||||||||||||
Reg. 573 Stand Pipes and branches-
Reg. 574 Stayed Flat surfaces (other than Crowns of Vertical Boilers). Stayed heads/ Braced and stayed surfaces.
| |||||||||||||||||||||||||
Images of the official Gazette pages that contain this regulation. Click to zoom. Compare word by word before relying on the extracted text.

Indian Boiler Regulations, 2026, reg. 464, Regulation 464, Gazette of India, Extraordinary, Part III—Section 4, No. 596, 1 October 2026, printed p.777. https://egazette.gov.in/WriteReadData/2026/276813.pdf (text consulted via IBRsource, 2026-11-23).
The citation refers to the government publication. Cite the Gazette, not this website.