Indian Boiler Regulations, 2026 · Chapter 12 · Shell Type Boilers of Welded Construction
Regulation 438. Cold bend tests
Not yet checked against the official Gazette; verify before relying on it.
438.Cold bend tests.─ (1) Two bend tests shall be made as given in this regulation.
(2)One specimen shall be tested with the outer surface of the weld in tension and the other with the inner surface in tension. The specimen shall be rectangular in section and shall be cut out transversely to the weld so as to have a width not less than one-and-a half times the thickness of the plates. The sharp corners of the specimens shall be rounded to a radius not exceeding 10% of the thickness of the specimen.
(3)Where the plate thickness does not exceed 32 mm, the thickness of the specimen shall be equal to the full thickness of the test plate. Where the plate thickness exceeds 32 mm, the specimen shall in all cases have a thickness of at least 32 mm. The specimen to be tested with the outer surface of the weld in tension shall be prepared by cutting to waste the metal local to the inner surface of the weld, so that the desired specimen thickness is obtained (see A, Figure 12/78).
(4)The specimen to be tested with the inner surface in tension shall be prepared by cutting to waste the metal local to the outer surface of the weld so that the desired specimen thickness is obtained (See B, Figure 12/78). Where the thickness of the plate permits, both specimens may be cut from the same piece of plate, the specimens being located in the plate one above the other (see C, Figure 12/78). Each specimen shall be mounted with the weld midway between the supports set apart at a distance of not more than 5.2 times the thickness of the specimen and pushed through the supports with a former having a diameter equal to three times the thickness of the specimen.
(5)On completion of the test, no crack or defect at the outer surface of the specimen shall be greater than 1.5 mm measured across the specimen or 3 mm measured along the length of the specimen. Premature failure at corners or the specimen shall not be considered cause for rejection.
Figures cited in this regulation (1, exact crops of the Gazette)

View Gazette page 819 · figure catalogue
Reconstructed CAD: DXF · SVG · Preview (redrawn, checked against the print; technical review pending)
In short
Sets how the two cold bend tests on Class I welded test plates are prepared, performed and judged.
Key points
- (1)–(2) Two specimens: one with the outer weld surface in tension, one with the inner surface in tension. They are rectangular, cut across the weld, at least one-and-a-half times the plate thickness wide, with corners rounded to a radius not over 10% of specimen thickness.
- (3) Plate not over 32 mm: specimen is the full test plate thickness. Over 32 mm: specimen at least 32 mm thick. The outer-surface specimen is made by cutting away metal near the inner surface (A, Figure 12/78).
- (4) The inner-surface specimen is made by cutting away metal near the outer surface (B, Figure 12/78). If thick enough, both may come from the same piece, one above the other (C).
- (4) The weld sits midway between supports no more than 5.2 times the specimen thickness apart, and is pushed through with a former of diameter three times the specimen thickness.
- (5) After the test, no crack or defect at the outer surface may exceed 1.5 mm across the specimen or 3 mm along its length.
Watch out
- Premature failure at the corners of the specimen is not a cause for rejection.
Written by IBRsource editors · last edited 2026-11-20. Explanations simplify and are not a design method, testing procedure or authorisation. Requirements come from the complete regulations, the Gazette and approved documentation.
Comparison pending: the IBR 1950 text in force on 30 September 2026 is not yet established for this provision, so no change is claimed (how this works).
Orientation hints (unverified)
These candidates come from automated heading matching against DPIIT's scanned historical print edition of IBR 1950. That edition uses imperial units and riveted-construction provisions, so it is not the operative 2026 predecessor text. Regulation numbers alone never prove equivalence.
| Historical 1950-edition reg. | Heading as OCR'd | Heading similarity | Source image |
|---|---|---|---|
| 19 | Bend Tests | 100% | Chapter II (DPIIT scan), image 2 |
| 84 | Bend Tests | 100% | Chapter II (DPIIT scan), image 16 |
| 262 | Bend Tests | 100% | Chapter V (DPIIT scan), image 7 |
Amendment history of the candidate IBR 1950 regulations: Reg. 19 (1 amendment)
IBR 1950 regulation 19 as last published in the DPIIT web edition (archived 2022)
Unofficial archived copy, not verified; see the regulation 19 page for its amendments.
| Reg. 19 MATERIALS OF CONSTRUCTION STEEL PLATES, RIVETS, SECTION AND BARS IN CARBON STEEL |
| Cold Bends.-(a) Test pieces shall be sheared lengthwise or crosswise from plates or bars, and shall not be less than 1½ inches wide, but for small bars the whole section may be used. For rivet bars bend tests are not required. b) In all cold bend tests, on samples 0.5 inch in thickness and above, the rough edge or arris caused by shearing may be removed by filing or grinding, and samples 1 inch in thickness and above may have the edges machined, but the test pieces shall receive no other preparation. The test pieces shall not be annealed unless the material from which they are cut is similarly annealed in which case the test piece shall be similarly and simultaneously treated with the material before testing. (c) (i) For bend test of plates of all grades of steel, the test piece shall withstands, without fracture, being bent cold through 180o around a mandrel, the radius of which shall have a relationship to the plate thickness as given below: Tensile strength Mandrel Radius 36 - 49 kg./mm2 1 T 41 - 57 kg./mm2 1 T 45 - 64 kg./mm2 1.5 T where T = Plate thickness (ii) For cold bend test of sections and bars, the test piece shall withstand, without fracture, being doubled over until the internal radius is equal to that shown in Table under regulation 16 and the limbs are parallel. (d) For small sectional material these bend tests may be made from the flattened bar. (e) Bend tests may be made either by pressure or by blows. |
IBR 1950 regulation 84 as last published in the DPIIT web edition (archived 2022)
Unofficial archived copy, not verified; see the regulation 84 page for its amendments.
| Reg. 84 MATERIALS OF CONSTRUCTION FORGED OR ROLLED PRESSURE PARTS OTHER THAN SEAMLESS DRUMS OF CARBON STEEL Bend Tests |
| (a) Bend test pieces shall be of rectangular cross section machined to a finished size of 1 inch wide by ¾ inch thick. In the case of headers, bend test pieces may be cut transversely 1½ T wide by T thick where T is the thickness of the header. The edges shall be rounded to a radius of 1/16 inch. The test pieces shall be bent over the thinner section. (b) Test pieces shall be bent when cold through an angle of 180° without fracture, the internal radius of the bend being not greater than that specified in table below for the 1 inch wide by ¾ inch thick test piece and not more than 1½ T for the full thickness test piece:
Bend tests may be made by pressure or by blows. |
IBR 1950 regulation 262 as last published in the DPIIT web edition (archived 2022)
Unofficial archived copy, not verified; see the regulation 262 page for its amendments.
|
| ||||||||||||||||||||||||||||||
Reg. 262 Bend Tests
Reg. 263
|
Images of the official Gazette pages that contain this regulation. Click to zoom. Compare word by word before relying on the extracted text.

Indian Boiler Regulations, 2026, reg. 438, Regulation 438, Gazette of India, Extraordinary, Part III—Section 4, No. 596, 1 October 2026, printed p.767. https://egazette.gov.in/WriteReadData/2026/276813.pdf (text consulted via IBRsource, 2026-11-23).
The citation refers to the government publication. Cite the Gazette, not this website.