Regulation 86. Flat end plates

Official text — not yet verifiedGazette 1 Oct 2026 · printed pp. 561–562

Not yet checked against the official Gazette; verify before relying on it.

Reproduced from the Gazette of India · verification status above

86. Flat end plates.─ (1) Wherever practicable, the flat or dished end plates of boilers shall be in one piece made from one rolled plate. Where diameter of boiler is so large as to make this impracticable, the flat end plates may be made from two pieces by fusion butt-welding. (See figures 12/1 and 12/2). In the latter case, the line of welding shall be parallel to the horizontal axis of the boiler and shall be subjected to full radiographic examination.

(2)Flanging of plates shall be done by machine. Cold forming of flanged end plate shall be followed by heat treatment. Such flanging shall be done hot, preferably in one operation, but where this is impracticable creep machine flanging may be used provided that the plate is worked at a suitable temperature and heated for an adequate distance beyond that portion of the plate under immediate treatment.

(3)Hot forming of welded plates shall be permitted provided that the welded joint is subjected to 100 percent radiographic or Ultrasonic examination after hot forming.

(4)Welded plates up to and including 20 mm thickness can be cold formed provided it complies with following conditions.

(a)Before cold forming, the weld reinforcement shall be ground smooth, and the manufacturer shall take precautions, where necessary, in order to avoid crack formation in the weld metal or the heat affected zone.

(b)If the inside radius of curvature after forming is less than 10 times the thickness, stress relieving shall be carried out.

(c)After cold forming, the welded joints shall be visually examined and subjected to 100 percent radiographic or Ultrasonic examination throughout their length. Joints of any thickness which have been cold formed to a radius less than 10 times the thickness.

(d)Knuckles shall be inspected for cracks by magnetic particle or penetrant methods.

(e)After completion of the flanging operation flanges shall be of true peripheral contour (either circular or straight as necessary to ensure accurate alignment with the connecting parts), and of good surface, free from bulges, grooves or other local irregularities; flat portions of the plate shall be free from set or distortion.

(5)In the construction of unfired boilers when the dished ends do not form a part of the heating surface cold spun dished ends conforming to IS: 2825 may be used.

(6)Care shall be taken to see that the flanges are circular and of good surface, free from local irregularities, and that they are parallel and square with the flat part of the plate.

(7)Flat portions of end plates, on completion of all flanging and machining operations, shall be flat and free from set or distortion.

Parts of this extracted text look garbled; read the Gazette page before using any value.

Figures cited in this regulation (2, exact crops of the Gazette)

Gazette Fig. 12/1
Fig. 12/1(no caption printed with this figure)
View Gazette page 798 · figure catalogue
Reconstructed CAD: DXF · SVG · Preview (redrawn, checked against the print; technical review pending)
Gazette Fig. 12/2
Fig. 12/2(no caption printed with this figure)
View Gazette page 798 · figure catalogue
Auto-traced outline: SVG · DXF (not to scale, may copy print defects)
Independent explanation — not the law · draft · engineer review in progress

In short

Regulation 86 covers how flat and dished end plates are made and formed: one-piece or welded construction, flanging, and hot and cold forming of welded plates.

Key points

  • (1) End plates should be one piece from one rolled plate wherever practicable. If the diameter is too large, flat end plates may be two pieces fusion butt-welded (Figures 12/1 and 12/2), with the weld line parallel to the boiler's horizontal axis and fully radiographed.
  • (2) Flanging is done by machine. Cold forming of a flanged end plate is followed by heat treatment. Flanging is done hot, preferably in one operation. Creep machine flanging is allowed if the plate is worked at a suitable temperature and heated well beyond the part being worked.
  • (3) Hot forming of welded plates is allowed if the weld gets 100 percent radiographic or ultrasonic examination after forming.
  • (4) Welded plates up to and including 20 mm thick may be cold formed if: the weld reinforcement is ground smooth first; stress relieving is done when the inside radius after forming is less than 10 times the thickness; welds are visually examined and get 100 percent radiographic or ultrasonic examination; knuckles are crack-checked by magnetic particle or penetrant methods; and flanges are true in contour, with flat portions free from set or distortion.
  • (5) For unfired boilers, cold spun dished ends to IS: 2825 may be used where they are not part of the heating surface.
  • (6), (7) Flanges must be circular, parallel and square with the flat part. Flat portions must be flat and free from set after all operations.

Watch out

  • The last sentence of (4)(c) appears incomplete in the extracted text. Check the Gazette page for its exact wording.

Written by IBRsource editors · last edited 2026-11-20. Explanations simplify and are not a design method, testing procedure or authorisation. Requirements come from the complete regulations, the Gazette and approved documentation.

Original drawings for this regulation

Comparison pending: the IBR 1950 text in force on 30 September 2026 is not yet established for this provision, so no change is claimed (how this works).

Orientation hints (unverified)

These candidates come from automated heading matching against DPIIT's scanned historical print edition of IBR 1950. That edition uses imperial units and riveted-construction provisions, so it is not the operative 2026 predecessor text. Regulation numbers alone never prove equivalence.

Historical 1950-edition reg.Heading as OCR'dHeading similaritySource image
33Plates100%Chapter II (DPIIT scan), image 3
113Flat End Plates100%Chapter III (DPIIT scan), image 2
429Unstayed Flat End Plates100%Chapter X (DPIIT scan), image 8

Amendment history of the candidate IBR 1950 regulations: Reg. 113 (1 amendment)

IBR 1950 regulation 33 as last published in the DPIIT web edition (archived 2022)

Unofficial archived copy, not verified; see the regulation 33 page for its amendments.

Reg. 33
MATERIALS OF CONSTRUCTION

COPPER PLATES, STAY AND RIVET BARS

Plates

(a) Process.- The copper shall be fire-refined or electrolytic and hot-rolled from suitable cakes.

(b) Chemical Composition.- The chemical composition of the plates shall be as follows:-

Per cent.
Copper 99.2 minimum
Arsenic .30 to .50
Antimony 0.05 maximum
Bismuth 0.05 maximum
Oxygen 0.10 maximum

(c) Freedom from defects.- The plates shall be clean, smooth and free from defects and shall have a workmanlike finish. They shall be thoroughly annealed.

(d) Rolling Margin.- No plate shall be under the specified thickness at any part, not more than 5% over the calculated weight. The scrap margin, partly sheared and left attached, shall be not less than 3 inches at the ends and 1½ inches at each side.

(e) Tensile Tests.- One tensile test shall be taken from each plate as rolled.

The tensile breaking strength, from Standard Test Piece A, shall not be less than 14 tons per sq. inch with an elongation of not less than 35%.

(f) Hot and Cold Bend tests.- One hot (temperature between 1200°F and 1400°F) and one cold bend test shall be taken from each plate as rolled.

For either hot or cold bend tests, the test piece shall withstand being doubled over without fracture until the sides are touching and parallel.

IBR 1950 regulation 113 as last published in the DPIIT web edition (archived 2022)

Unofficial archived copy, not verified; see the regulation 113 page for its amendments.

Reg. 113
END PLATES
Flat End Plates

a) The plates of boilers shall preferably be in one piece made from one rolled plate. Alternatively, the end plates may be built up from two pieces by riveting or by fusion butt-welding. In the latter case, the line of weld shall be parallel to the horizontal axis of the boiler and the entire plate after flanging shall be subjected to stress relieving and the weld shall be radiographed.
b) The peripheral flanging of end plates shall be done by machine. Such flanging shall preferably be done in one operation, but where this is impracticable sectional or creep machine flanging may be permitted, provided that the plate is worked at a suitable temperature, and the plate is heated to an adequate distance beyond the portion under immediate treatment.
bb) In the construction of unfired boilers when the dished ends do not form a part of the heating surface, cold spun dished ends conforming to IS: 2825 may be used.
c) Care must be taken to see that the flanges are circular and of good surface, free from local irregularities, and that they are parallel and square with the flat part of the plate. For the purpose of relieving internal stresses, all plates which have been flanged or locally heated shall afterwards be efficiently annealed unless during the last stage of manufacture they have been uniformly heated throughout.
d) Flat portions of end plates, on completion of all flanging and machining operations, shall be flat and free from set or distortion.

IBR 1950 regulation 429 as last published in the DPIIT web edition (archived 2022)

Unofficial archived copy, not verified; see the regulation 429 page for its amendments.

Reg. 427, Reg. 428, Reg. 429, Reg. 430
TESTS FOR CLASS II FUSION WELDED SEAMS

Manholes and other openings in Shells

Manholes and other openings in boiler shells shall be placed away from any welded seam. Oval openings shall be arranged with their minor axis parallel to the longitudinal centre line of the boiler.

(a) Un-compensated openings shall comply with Regulation 187.
(b) Compensated openings shall comply with Regulations 170, 171, 186 and 279.


Reg. 428
TESTS FOR CLASS II FUSION WELDED SEAMS

Dished End Plates with pressure on Concave side

This shall comply with Regulation 408.



Reg. 429
TESTS FOR CLASS II FUSION WELDED SEAMS

Unstayed Flat End Plates

The working pressure of unstayed flat end plates shall comply with Regulation 412.

Where the diameter of the openings in an unstayed flat end plate is greater than 2½ inches or the pitch in inches is less than four times the diameter of the holes full compensation shall be provided as in Regulation 279.



Reg. 430
TESTS FOR CLASS II FUSION WELDED SEAMS

Thickness of Angle Rings

Thickness of angle rings shall comply with Regulation 379(a).

Images of the official Gazette pages that contain this regulation. Click to zoom. Compare word by word before relying on the extracted text.

Instrument
Indian Boiler Regulations, 2026 (made by the Central Boilers Board under s.40 of the Boilers Act, 2025)
Notification
F.No. P-30014/3/2021-Boiler dated 7 Aug 2026
Published
Gazette of India, Extraordinary, Part III Sec. 4, No. 596, 1 Oct 2026 (CG-DL-E-06102026-276813)
In force
1 Oct 2026 (reg. 1(3): date of publication in the Official Gazette)
Printed Gazette page
561–562
PDF page index
561–562 · open official e-Gazette PDF
Extraction
pdftotext layout mode, sequential regulation detector · text hash e7dc08710f1f3071
Verification
Official text — not yet verified
Amendments checked
None known after 1 Oct 2026 as of build date (not a guarantee). Amendment log
How to cite

Indian Boiler Regulations, 2026, reg. 86, Regulation 86, Gazette of India, Extraordinary, Part III—Section 4, No. 596, 1 October 2026, printed p.561–562. https://egazette.gov.in/WriteReadData/2026/276813.pdf (text consulted via IBRsource, 2026-11-23).

The citation refers to the government publication. Cite the Gazette, not this website.

Help improve this page

Engineers like you keep IBRsource accurate. Every checked correction or tip helps the next reader.