Indian Boiler Regulations, 2026 · Chapter 4 · Fusion Welded Drums for Water Tube Boilers and Superheaters
Regulation 159. Tensile tests
Not yet checked against the official Gazette; verify before relying on it.
159. Tensile tests.─(1)The tensile strength of different grades of material shall be within the limits specified in regulation 37.
(2)The upper yield point at room temperature shall be not less than 50% of the specified minimum tensile strength at room temperature.
(3)The breaking elongation in percentage shall be not less than (N-Rm)/C Where Rm = Tensile strength at room temperature in kgf/mm2
N = a quality index of 100 for plate thickness upto 50 mm or 95 for plate thickness over 50mm.
C = 2.2 for only gauge lengths of Lο= 5 do or Lο=5.65/ √ Aο
Where Lο = gauge length
Aο = original cross section of the rectangular test piece.
do = original diameter of the round test piece.
NOTE: C= 1.9 for gauge lengths of 4 √ Aο for test piece of Appendix-D.
(4)The minimum values of the stress at proof limit 0.2% at elevated temperature (Et) may be calculated by multiplying the minimum specified tensile strength at room temperature (R20) by the value of the ratio (Et/R20) given in the Table 2/5 in regulation 37.
Tables and formulae are shown in their extracted layout. Alignment, superscripts and subscripts may be lost. The Gazette page image is authoritative.
In short
Regulation 159 sets the acceptance requirements for tensile tests on fusion welded joints.
Key points
- (1) Tensile strength must be within the limits in regulation 37.
- (2) Upper yield point at room temperature must be at least 50% of the specified minimum tensile strength.
- (3) Breaking elongation (%) must be at least (N-Rm)/C. Rm is tensile strength in kgf/mm²; N is 100 for plate up to 50 mm or 95 over 50mm; C is 2.2 for the gauge lengths stated, or 1.9 for the gauge length in the Note.
- (4) Minimum 0.2% proof stress at elevated temperature (Et) may be found by multiplying the room temperature minimum tensile strength (R20) by the Et/R20 ratio in Table 2/5 of regulation 37.
Written by IBRsource editors · last edited 2026-11-20. Explanations simplify and are not a design method, testing procedure or authorisation. Requirements come from the complete regulations, the Gazette and approved documentation.
Comparison pending: the IBR 1950 text in force on 30 September 2026 is not yet established for this provision, so no change is claimed (how this works).
Orientation hints (unverified)
These candidates come from automated heading matching against DPIIT's scanned historical print edition of IBR 1950. That edition uses imperial units and riveted-construction provisions, so it is not the operative 2026 predecessor text. Regulation numbers alone never prove equivalence.
| Historical 1950-edition reg. | Heading as OCR'd | Heading similarity | Source image |
|---|---|---|---|
| 17 | Number of Tensile Tests | 100% | Chapter II (DPIIT scan), image 2 |
| 83 | Tensile Tests | 100% | Chapter II (DPIIT scan), image 16 |
| 260 | Tensile Tests | 100% | Chapter V (DPIIT scan), image 6 |
Amendment history of the candidate IBR 1950 regulations: Reg. 17 (3 amendments) · Reg. 260 (1 amendment)
IBR 1950 regulation 17 as last published in the DPIIT web edition (archived 2022)
Unofficial archived copy, not verified; see the regulation 17 page for its amendments.
| Reg. 17 MATERIALS OF CONSTRUCTION STEEL PLATES, RIVETS, SECTION AND BARS IN CARBON STEEL |
| (a) Plates – For shell plates, butt straps and plates, gusset plates, end plates, furnace plates and flanging plates one tensile test piece shall be cut from each plate as rolled. (b) Angle, tee, rivet, and stay bars.- One tensile test shall be made from each 15 or part of 15 bars rolled of each section or diameter from the same charge, but not less than two tensile tests shall be made unless the total number of bars rolled from the same charge is 8 or less than 8 and the bars of the same section or diameter, in which case one tensile test shall suffice. For round bars of 1¾ inches diameter and under, the numbers 50 and 20 shall be substituted for 15 and 8 respectively for determining the number of tests required. |
IBR 1950 regulation 83 as last published in the DPIIT web edition (archived 2022)
Unofficial archived copy, not verified; see the regulation 83 page for its amendments.
| Reg. 83 MATERIALS OF CONSTRUCTION FORGED OR ROLLED PRESSURE PARTS OTHER THAN SEAMLESS DRUMS OF CARBON STEEL Tensile strength |
| (a) The tensile strength of the material shall conform to one of the following four grades:- (i) 37 to 45 kgf/mm2 (b) The upper yield point at room temperature shall be not less than 50% of the specified minimum tensile strength. (c) The minimum values of the stress at proof limit 0.2% at elevated temperature Et of the material may be calculated by multiplying the minimum specified tensile strength at room temperature R20 by the value of the ratio Et/R20 given in the table under Regulation 16. (d) The breaking elongation in percentage shall not be less than
|
IBR 1950 regulation 260 as last published in the DPIIT web edition (archived 2022)
Unofficial archived copy, not verified; see the regulation 260 page for its amendments.
|
| ||||||
Reg. 260
(b) All-weld Metal
|
Images of the official Gazette pages that contain this regulation. Click to zoom. Compare word by word before relying on the extracted text.

Indian Boiler Regulations, 2026, reg. 159, Regulation 159, Gazette of India, Extraordinary, Part III—Section 4, No. 596, 1 October 2026, printed p.592. https://egazette.gov.in/WriteReadData/2026/276813.pdf (text consulted via IBRsource, 2026-11-23).
The citation refers to the government publication. Cite the Gazette, not this website.