Indian Boiler Regulations, 2026 · Chapter 4 · Fusion Welded Drums for Water Tube Boilers and Superheaters
Regulation 160. Bend test pieces
Not yet checked against the official Gazette; verify before relying on it.
160. Bend test pieces.─(1)One for direct and one for reverse bending shall be taken transversely to the weld and where the thickness of the plate permits, one should be above the other. The specimens shall be rectangular in section so as to have width equal to one and half times the thickness of the specimen but not less than 30 mm. The surface of the specimens shall be machined just to remove the surface irregularities of the plate and the weld. The corners of the specimens shall be rounded to a radius not exceeding 10% of the thickness of the specimen.
(2)Where plate thicknesses do not exceed 38 mm, the thickness of the specimen shall be equal to the full thickness of the test plate. Where the plate thickness exceeds 38 mm, the specimen shall in all cases have a thickness of at least 38 mm. The specimen to be tested with the outer surface of the weld in tension shall be prepared by cutting to waste the metal local to the inner surface of the weld so that the desired specimen thickness is obtained (see Fig.4/6, Specimen A). The specimen to be tested with the inner surface in tension shall be prepared by cutting to waste the metal local to the outer surface of the weld so that the desired specimen thickness is obtained (see Fig. 4/6, Specimen B). Where the thickness of the plate permits, both specimens may be cut from the same piece of plate, the specimen being located in the plate one above the other (see Fig. 4/6, Specimen C).
All dimensions are in mm.
Fig. 4/6: Specimen Three Bend Test
Figures cited in this regulation (1, exact crops of the Gazette)

View Gazette page 593 · figure catalogue
Reconstructed CAD: DXF · SVG · Preview (redrawn, checked against the print; technical review pending)
In short
Regulation 160 sets how bend test specimens are taken and prepared.
Key points
- (1) One direct and one reverse bend specimen, taken across the weld, one above the other where thickness permits. Width is one and a half times specimen thickness, but not less than 30 mm. Surfaces are machined just to remove irregularities; corner radius not more than 10% of thickness.
- (2) Up to 38 mm plate, specimen thickness equals the full plate thickness. Over 38 mm, specimens are at least 38 mm thick, cut from the outer side (outer surface in tension, Specimen A) or inner side (inner surface in tension, Specimen B), or both from the same piece one above the other (Specimen C), as in Fig. 4/6.
Written by IBRsource editors · last edited 2026-11-20. Explanations simplify and are not a design method, testing procedure or authorisation. Requirements come from the complete regulations, the Gazette and approved documentation.
Comparison pending: the IBR 1950 text in force on 30 September 2026 is not yet established for this provision, so no change is claimed (how this works).
Orientation hints (unverified)
These candidates come from automated heading matching against DPIIT's scanned historical print edition of IBR 1950. That edition uses imperial units and riveted-construction provisions, so it is not the operative 2026 predecessor text. Regulation numbers alone never prove equivalence.
| Historical 1950-edition reg. | Heading as OCR'd | Heading similarity | Source image |
|---|---|---|---|
| 419 | Bend Test | 100% | Chapter X (DPIIT scan), image 7 |
| 14 | Selection of test pieces | 81% | Chapter II (DPIIT scan), image 1 |
| 82 | Selection of test pieces | 81% | Chapter II (DPIIT scan), image 16 |
Amendment history of the candidate IBR 1950 regulations: Reg. 14 (1 amendment) · Reg. 82 (1 amendment)
IBR 1950 regulation 419 as last published in the DPIIT web edition (archived 2022)
Unofficial archived copy, not verified; see the regulation 419 page for its amendments.
| Reg. 418, Reg. 419
Reg. 419
|
IBR 1950 regulation 14 as last published in the DPIIT web edition (archived 2022)
Unofficial archived copy, not verified; see the regulation 14 page for its amendments.
| Reg. 14 MATERIALS OF CONSTRUCTION STEEL PLATES, RIVETS, SECTION AND BARS IN CARBON STEEL |
| All test pieces shall be selected by the Inspecting Officer and tested in his presence, and he shall satisfy himself that the conditions herein described are fulfilled. |
IBR 1950 regulation 82 as last published in the DPIIT web edition (archived 2022)
Unofficial archived copy, not verified; see the regulation 82 page for its amendments.
| Reg. 82 MATERIALS OF CONSTRUCTION FORGED OR ROLLED PRESSURE PARTS OTHER THAN SEAMLESS DRUMS OF CARBON STEEL Selection of test pieces |
| (a) For testing, either the parts themselves shall be used or additional material of sufficient size for test pieces shall be available. In the case of headers for example, surplus lengths for test rings may be used. In the case of flanges swaged in dies, the punching left may be used as test pieces in which case the identity of the material of the punching with that of the flange shall be evidenced in an adequate manner. The test may be performed also on the semi-finished material for example a bar or a billet, provided it is given approximately the same reduction and heat-treatment as the finished forgings. For headers with closed ends, the test rings shall be cut off before dishing or reducing and shall be subjected to the same heat treatment as the headers themselves. In the case of headers which are closed by special covers, the test ring shall be cut off after heat-treatment. Similar procedures shall be followed for test pieces of other forgings. (b) For testing, piece of one and the same cast of the same heat treatment batch as well as of similar dimensions may be gathered into one group. At least one test piece shall be made from each group. (c) A proportional test piece with Lo = 5 do shall be used as a test specimen. (d) Tangential test piece shall be used for headers where practicable. For headers with outside diameter less than 200 mm longitudinal test pieces may be allowed. (e) Hydraulic Test.- A hydraulic test shall be carried out at the Maker’s works in accordance with the requirements of regulation 268, if required by the Inspecting Authority. |
Images of the official Gazette pages that contain this regulation. Click to zoom. Compare word by word before relying on the extracted text.


Indian Boiler Regulations, 2026, reg. 160, Regulation 160, Gazette of India, Extraordinary, Part III—Section 4, No. 596, 1 October 2026, printed p.592–593. https://egazette.gov.in/WriteReadData/2026/276813.pdf (text consulted via IBRsource, 2026-11-23).