Indian Boiler Regulations, 2026 · Chapter 11 · Standard Conditions for the Design and Construction of Economisers, Feed Pipes, Feed Heaters and Other Similar Vessels

Regulation 364. Test bars

Official text — not yet verifiedGazette 1 Oct 2026 · printed pp. 744–745

Not yet checked against the official Gazette; verify before relying on it.

Reproduced from the Gazette of India · verification status above

364.Test bars.─ (1) (a)When test bars are cast separately, they shall be poured at the same time and from the same ladle of metal as the casting or castings they represent.

(b)The number of test bars specified in regulation 365 shall be applicable to all casting of each melt.

(2)When the bars are cast on the mould for the casting and the mould for the test piece shall be joined together in such a manner that the liquid metal fills both moulds at the same operation.

(3)All test bars shall be cast in the same type of sand moulds viz. green sand or in loam or dry sand as used in casting or castings they represent.

(4)The test bar shall not be subjected to any heat treatment after leaving the moulds except where the castings are heat treated.

Referenced provisions

Reg. 365

Independent explanation — not the law · draft · engineer review in progress

In short

Regulation 364 sets how test bars for economiser castings are cast, so that they truly represent the castings.

Key points

  • (1)(a) Separately cast test bars must be poured at the same time and from the same ladle as the castings they represent.
  • (1)(b) The number of test bars in regulation 365 applies to all castings of each melt.
  • (2) Where bars are cast on the casting's mould, the two moulds must be joined so the liquid metal fills both in the same operation.
  • (3) Test bars must be cast in the same type of sand mould (green sand, loam or dry sand) as the castings.

Watch out

  • (4) Test bars must not be heat treated after leaving the moulds, except where the castings themselves are heat treated.

Written by IBRsource editors · last edited 2026-11-20. Explanations simplify and are not a design method, testing procedure or authorisation. Requirements come from the complete regulations, the Gazette and approved documentation.

Comparison pending: the IBR 1950 text in force on 30 September 2026 is not yet established for this provision, so no change is claimed (how this works).

Orientation hints (unverified)

These candidates come from automated heading matching against DPIIT's scanned historical print edition of IBR 1950. That edition uses imperial units and riveted-construction provisions, so it is not the operative 2026 predecessor text. Regulation numbers alone never prove equivalence.

Historical 1950-edition reg.Heading as OCR'dHeading similaritySource image
507Test bars100%Chapter XI (DPIIT scan), image 2
30Stay Bars78%Chapter II (DPIIT scan), image 3
31Stay Bars78%Chapter II (DPIIT scan), image 3
IBR 1950 regulation 507 as last published in the DPIIT web edition (archived 2022)

Unofficial archived copy, not verified; see the regulation 507 page for its amendments.


Reg. 507, Reg. 508
STANDARD CONDITIONS FOR THE DESIGN AND CONSTRUCTION OF ECONOMISER, FEED PIPES, FEED HEATERS AND OTHER SIMILAR VESSELS

CAST IRON, TUBES AND HEADERS

Test bars

For all new economisers the hydraulic test must be applied as shown below:-

a) When the test bars are cast separately, they shall be poured at the same time and from the same ladle of metal as the casting or castings they represent. The number of test bars specified in Regulation 508 shall be applicable to all castings of each melt.
b) when the bars are cast on the mould for the castings and the mould for the test piece shall be joined together in such a manner that the liquid metal fills both moulds at the same operation.
c) all test bars shall be cast in green sand or in loam or dry sand moulds according as to whether the casting or castings they represent are moulded in green sand, or in loam or dry sand respectively.
d) The test bars shall not be subjected to any heat treatment after leaving the moulds except where the castings are heat-treated.



Reg. 508
STANDARD CONDITIONS FOR THE DESIGN AND CONSTRUCTION OF ECONOMISER, FEED PIPES, FEED HEATERS AND OTHER SIMILAR VESSELS

CAST IRON, TUBES AND HEADERS

Number of tensile tests

(a) The number of tests required for each batch of castings shall be in accordance with the following table the various classes of castings being divided into 4 representative groups:-

Group Weight of castings Test requirements
1. Up to 28 lbs One test for each 30 cwts. Of castings or part thereof.


One test for each 2 tons of castings or part thereof.

2. Over 28 lbs. and up to 1 cwt
3. Over 1 cwt. And up to 1 ton One test for each 3 tons of castings or part thereof.
 

In the above Group 1, 2 and 3, all castings represented by one test must be poured from the same ladle of same heat as the bar or bars provided for the test.

4. Over 1 ton and important castings One test for each 4 tons of castings or part thereof or for each casting weighing 4 tons or more.

(b) Conditions for Acceptance and for Rejection:-

Test Result Conclusion
1st Pass The batch or separate casting represented shall be accepted.
Tensile or Transverse test fails Two more tests shall be made.
2nd If both pass
If  either fails 
The batch or separate casting represented shall be accepted.
The batch or separate castings represented shall be rejected.

Provided always that, in the case of failure of any test piece showing obvious casting defects, another test piece shall be taken from spare test bars or cut from a casting from the same batch and the results obtained from this substituted for those obtained from the defective test bars.

IBR 1950 regulation 30 as last published in the DPIIT web edition (archived 2022)

Unofficial archived copy, not verified; see the regulation 30 page for its amendments.

Reg. 30
MATERIALS OF CONSTRUCTION

WROUGHT IRON STAY AND RIVET BARS

Stay Bars

The tensile breaking strength shall be between 21 and 25 tons with an elongation of not less than 22 per cent measured on the Standard Test Piece B or 27 per cent measured on the Standard Test Piece B1.
IBR 1950 regulation 31 as last published in the DPIIT web edition (archived 2022)

Unofficial archived copy, not verified; see the regulation 31 page for its amendments.

Reg. 31
MATERIALS OF CONSTRUCTION

WROUGHT IRON STAY AND RIVET BARS

Stay Bars - Bend Tests

To comply with  Regulation 19.

Images of the official Gazette pages that contain this regulation. Click to zoom. Compare word by word before relying on the extracted text.

Instrument
Indian Boiler Regulations, 2026 (made by the Central Boilers Board under s.40 of the Boilers Act, 2025)
Notification
F.No. P-30014/3/2021-Boiler dated 7 Aug 2026
Published
Gazette of India, Extraordinary, Part III Sec. 4, No. 596, 1 Oct 2026 (CG-DL-E-06102026-276813)
In force
1 Oct 2026 (reg. 1(3): date of publication in the Official Gazette)
Printed Gazette page
744–745
PDF page index
744–745 · open official e-Gazette PDF
Extraction
pdftotext layout mode, sequential regulation detector · text hash 4ea5945952e65f6a
Verification
Official text — not yet verified
Amendments checked
None known after 1 Oct 2026 as of build date (not a guarantee). Amendment log
How to cite

Indian Boiler Regulations, 2026, reg. 364, Regulation 364, Gazette of India, Extraordinary, Part III—Section 4, No. 596, 1 October 2026, printed p.744–745. https://egazette.gov.in/WriteReadData/2026/276813.pdf (text consulted via IBRsource, 2026-11-23).