BETAIndependent engineering reference. Source-text verification is ongoing.Verification ongoing.Verification status →
IBRsourceIndian Boiler Regulations, made clear

Indian Boiler Regulations, 2026 · Chapter 10 · Electrode Boilers

Regulation 340. Bend Test

Official text — not yet verifiedGazette 1 Oct 2026 · printed p. 734Figure referenced

Not yet checked against the official Gazette; verify before relying on it.

Reproduced from the Gazette of India · verification status above

340. Bend Test.─ (1) (a) Two bend tests shall be made for welded seams.

(b)One specimen shall be tested with the outer surface or the weld in tension, and the other with the inner surface in tension.

(c)The specimen shall be rectangular in section and shall be cut out transversely to the weld so as to have a width of not less than 1½ times the thickness of the plate.

(d)The sharp corners of the specimens shall be rounded to a radius not exceeding ten percent of the thickness of the specimen.

(2)(a) Where the plate thickness does not exceed 32 mm, the thickness of the specimen shall be equal to the full thickness of the test plate.

(b)Where the plate thickness exceeds 32 mm, the thickness of the specimen shall be at least 32 mm.

(c)The specimen to be tested with the outer surface of the weld in tension shall be prepared by cutting to waste the metal local to the inner surface of the weld, so that the desired specimen thickness is obtained.

(3)(a) The specimen to be tested with the inner surface in tension shall be prepared by cutting to waste the metal local to the outer surface of the weld so that the desired metal thickness is obtained.

(b)Where the thickness of the plate permits, both specimen being located in the plate one above the other.

(c)Each specimen shall be mounted with the weld midway between the support, set apart at a distance of not more than 5.2 times the thickness of the specimen and pushed through the supports with a former having a diameter equal to three times the thickness of the specimen (see Fig. 4/6 of regulation 160 of chapter 4).

(4)(a) On completion of the test, no crack or defect at the outer surface of the specimen shall be greater than

1.5 mm, measured across the specimen or 3 mm measured along the length of the specimen.

(b)Premature failure at corners of the specimen shall not be considered cause for rejection (see Fig. 4/6, specimen A).

Referenced provisions

Reg. 160

Figures cited in this regulation (1, exact crops of the Gazette)

Gazette Fig. 4/6: Specimen Three Bend Test
Fig. 4/6Specimen Three Bend Test
View Gazette page 593 · figure catalogue
Reconstructed CAD: DXF · SVG · Preview (redrawn, checked against the print; technical review pending)
Independent explanation — not the law · draft · engineer review in progress

In short

Regulation 340 sets the two bend tests for welded seams of fusion welded electrode boilers: how specimens are prepared, how they are bent and what defects are allowed.

Key points

  • (1) Two bend tests: one with the outer surface of the weld in tension, one with the inner surface in tension. Specimens are rectangular, cut transversely to the weld, at least 1½ times the plate thickness wide, with corners rounded to a radius not exceeding ten percent of the specimen thickness.
  • (2) Plate thickness up to 32 mm: specimen thickness equals full plate thickness. Over 32 mm: specimen at least 32 mm thick. For the outer-surface test, metal near the inner surface is cut to waste.
  • (3) For the inner-surface test, metal near the outer surface is cut to waste. Where thickness permits, both specimens may be taken one above the other. The weld sits midway between supports set not more than 5.2 times the specimen thickness apart, and is pushed through with a former of diameter three times the specimen thickness (see Fig. 4/6 of regulation 160).
  • (4)(a) After the test, no crack or defect on the outer surface may exceed 1.5 mm across the specimen or 3 mm along its length.

Watch out

  • (4)(b) Premature failure at the corners of the specimen is not a cause for rejection.

Written by IBRsource editors · last edited 2026-11-20. Explanations simplify and are not a design method, testing procedure or authorisation. Requirements come from the complete regulations, the Gazette and approved documentation.

Comparison pending: the IBR 1950 text in force on 30 September 2026 is not yet established for this provision, so no change is claimed (how this works).

Orientation hints (unverified)

These candidates come from automated heading matching against DPIIT's scanned historical print edition of IBR 1950. That edition uses imperial units and riveted-construction provisions, so it is not the operative 2026 predecessor text. Regulation numbers alone never prove equivalence.

Historical 1950-edition reg.Heading as OCR'dHeading similaritySource image
3Bend test, outef and inner surfaces of plate (at weld)100%Chapter V (DPIIT scan), image 5
419Bend Test100%Chapter X (DPIIT scan), image 7
19Bend Tests95%Chapter II (DPIIT scan), image 2

Amendment history of the candidate IBR 1950 regulations: Reg. 3 (6 amendments) · Reg. 19 (1 amendment)

IBR 1950 regulation 3 as last published in the DPIIT web edition (archived 2022)

Unofficial archived copy, not verified; see the regulation 3 page for its amendments.

Reg. 3
General Requirements, Application of Standard Conditions and Exceptions thereto:

3(1) A boiler shall not be registered under sub-section (4) of Section 7 of the Act and a certificate shall not be issued under sub-section (5) of that section with reference to a boiler, unless the standard conditions in respect of material, design and construction, which are specified in the subsequent Chapters of these Regulations, are satisfied in respect of such a boiler.

(2) Notwithstanding anything contained in sub-regulation (1), the Chief Inspector may, subject to the provisions of regulation 7 and 8, register a boiler and order the issue of a certificate authorising the use thereof, under any of the following circumstances, namely -

(i) when the material used in the construction of a boiler, steam-pipe, economiser or superheater is not in conformity with the Indian Boiler Regulations but is known to be commonly used in other countries as being suitable for use in the construction of boilers and steam-pipes, provided that such material is not specifically prohibited by the Regulation and that the methods of manufacture, fabrication and heat treatment conform to the specified Codes or Standards;
(ii) when the constructional features of a boiler, steam-pipe, economiser or superheater are not in conformity with the Regulations but are not considered by the Chief Inspector to be inferior in strength to those prescribed in the Regulations and form part of the usual manufacturing practice of boilers and steam-pipes in other countries;
(iii) when a boiler, steam-pipe, economiser or superheater has obviously been built in conformity with the regulations but no certificate as required under the regulations is forthcoming.

(3) No structural part of a boiler, which is subject to pressure, shall be made of Bessemer process steel or of Cast or Malleable Cast Iron.

(4) Where no specific provision is made in these regulations for design or manufacture of any pressure part, the Inspecting Authority may permit the design, manufacture, stage inspections and certification of such pressure parts including the valves, mountings and fittings conforming to the Codes or Standards like BS, ASME Boiler and pressure vessels code, TEMA, TRD, GOST and JIS which are known to be commonly used in industrially advanced countries. The decision of Inspecting Authorities shall be binding on all Registering authorities.

(4A) The tubes of  boilers  and  heat exchangers  made of  Titanium  and other exotic metals may be approved as per international codes, including ASME, BS, DIN, TEMA  with the minimum thickness specified in those codes of manufacture.


IBR 1950 regulation 419 as last published in the DPIIT web edition (archived 2022)

Unofficial archived copy, not verified; see the regulation 419 page for its amendments.

Reg. 418, Reg. 419
TESTS FOR CLASS II FUSION WELDED SEAMS

Tensile test

The specimen shall be cut out transversely to the welded seam (see Figure 50) and shall be of the full thickness of the plate at the welded seam and the breadth W shall be as great as the testing machine will reasonably allow provided the effective cross-sectional areas is not less than 1 ½ sq. in. (see fig. 51). The ultimate tensile stress of the welded seam specimen shall be not less than the lower limit specified for the plate (see Table under Regulation 16).



Reg. 419
TESTS FOR CLASS II FUSION WELDED SEAMS

Bend Test

Two bend tests shall be made.

One specimen shall be tested with the outer surface or the weld in tension, and the other with the inner surface in tension. The specimens shall be rectangular in section and shall be cut out transversely to the weld so as to have a width of not less than one-and-a-half times the thickness of the plate. The sharp corners of the specimens shall be rounded to a radius not exceeding ten per cent of the thickness of the specimen.

Where the plate thickness does not exceed 1 ¼ inches the thickness of the specimen shall be equal to the full thickness of the test plate. Where the plate thickness exceeds 1 ¼ inches the thickness of the specimen shall be at least 1 ¼ inches. The specimen to be tested with the outer surface of the weld in tension shall be prepared by cutting to waste the metal local to the inner surface of the weld, so that the desired specimen thickness is obtained.

The specimen to be tested with the inner surface in tension shall be prepared by cutting to waste the metal local to the outer surface of the weld so that the desired metal thickness is obtained. Where the thickness of the plate permits, both specimens may be cut from the same piece of plate, the specimens being located in the plate one above the other. Each specimen shall be mounted with the weld midway between the supports, set apart at a distance of not more than 5.2 times the thickness of the specimen and pushed through the support with a former having a diameter equal to three times the thickness of the specimen( see Fig 20).

One completion of the test no crack or defect at the outer surface of the specimen shall be greater than 1/16 inch measured across the specimen or 1/8 inch measured along the length of the specimen. Premature failure at corner of the specimen shall not be considered cause for rejection ( see Fig 20, Specimen A.)

IBR 1950 regulation 19 as last published in the DPIIT web edition (archived 2022)

Unofficial archived copy, not verified; see the regulation 19 page for its amendments.

Reg. 19
MATERIALS OF CONSTRUCTION

STEEL PLATES, RIVETS, SECTION AND BARS IN CARBON STEEL

Bend Tests

Cold Bends.-(a) Test pieces shall be sheared lengthwise or crosswise from plates or bars, and shall not be less than 1½ inches wide, but for small bars the whole section may be used. For rivet bars bend tests are not required.

b) In all cold bend tests, on samples 0.5 inch in thickness and above, the rough edge or arris caused by shearing may be removed by filing or grinding, and samples 1 inch in thickness and above may have the edges machined, but the test pieces shall receive no other preparation. The test pieces shall not be annealed unless the material from which they are cut is similarly annealed in which case the test piece shall be similarly and simultaneously treated with the material before testing. 

(c) (i) For bend test of plates of all grades of steel, the test piece shall withstands, without fracture, being bent cold through 180o around a mandrel, the radius of which shall have a relationship to the plate thickness as given below:

      Tensile strength                          Mandrel Radius

      36 - 49 kg./mm2                              1 T

      41 - 57 kg./mm2                              1 T

      45 - 64 kg./mm2                            1.5 T

where T = Plate thickness  

(ii) For cold bend test of sections and bars, the test piece shall withstand, without fracture, being doubled over until the internal radius is equal to that shown in Table under regulation 16 and the limbs are parallel.

(d) For small sectional material these bend tests may be made from the flattened bar.

(e) Bend tests may be made either by pressure or by blows.

Images of the official Gazette pages that contain this regulation. Click to zoom. Compare word by word before relying on the extracted text.

Instrument
Indian Boiler Regulations, 2026 (made by the Central Boilers Board under s.40 of the Boilers Act, 2025)
Notification
F.No. P-30014/3/2021-Boiler dated 7 Aug 2026
Published
Gazette of India, Extraordinary, Part III Sec. 4, No. 596, 1 Oct 2026 (CG-DL-E-06102026-276813)
In force
1 Oct 2026 (reg. 1(3): date of publication in the Official Gazette)
Printed Gazette page
734
PDF page index
734 · open official e-Gazette PDF
Extraction
pdftotext layout mode, sequential regulation detector · text hash baac860d886b32ac
Verification
Official text — not yet verified
Amendments checked
None known after 1 Oct 2026 as of build date (not a guarantee). Amendment log
How to cite

Indian Boiler Regulations, 2026, reg. 340, Regulation 340, Gazette of India, Extraordinary, Part III—Section 4, No. 596, 1 October 2026, printed p.734. https://egazette.gov.in/WriteReadData/2026/276813.pdf (text consulted via IBRsource, 2026-11-23).

The citation refers to the government publication. Cite the Gazette, not this website.

Help improve this page

Engineers like you keep IBRsource accurate. Every checked correction or tip helps the next reader.