BETAIndependent engineering reference. Source-text verification is ongoing.Verification ongoing.Verification status →
IBRsourceIndian Boiler Regulations, made clear

Indian Boiler Regulations, 1950 (superseded 1 Oct 2026)

Regulation 611

Unofficial DPIIT web edition · not verified2 amendments found

Text in the DPIIT web edition

Archived copy captured 05 Aug 2022 (Wayback Machine); the same page also prints regulations 610, 611A, 611B. The text matches the 2019 capture; amendments from 2020 onwards are probably not included. Units as printed.

Unofficial DPIIT web edition · archived 2022 · not checked against the Gazette

Reg. 610, Reg. 611 A, Reg. 611 B

QUALIFICATION TESTS FOR WELDERS ENGAGED IN WELDING OF BOILERS AND STEAM-PIPES UNDER CONSTRUCTION, ERECTION AND FABRICATION AT SITE IN INDIA AND IN REPAIRING BOILERS AND STEAM-PIPES BY WELDING

Reg 610

Tests for Requalification

At a requalification test a welder need not be examined in theoretical subjects, but he shall be required to qualify in the following practical tests:-

a) Plate Welding.-

A groove welded joint of two pieces of plates not less than 16 mm. (5/8 inch) thick over a length of 152 mm. (6 inches) in a position 45 degree to vertical, size of plates to be welded being 229 mm. x 152 mm. (9 inches x 6 inches). The main welding is to be carried from the underside only.
(b) Pipe Welding.-

The material of plates, tubes, pipes and electrodes used for these tests shall conform to the requirements of appropriate Regulations as may be applicable in each case.
(i) A groove welded joint with the axis of the pipe in a horizontal position and without rotating the pipe.
(ii) One weld of a branch to a pipe, as prescribed in Regulation 609.
(c)

(d)

Tube Welding.-

A butt welded joint of two pieces of boiler tubes with the axis in a vertical position, and tubes of same size fixed in adjoining positions. This test shall be in addition to the test for pipe welding under clause (b).

When a welder is continuously engaged on production weld, tests on the work in actual production to the satisfaction of the Competent Authority may be accepted as an alternative to the tests prescribed as above under clauses (a), (b) and (c).



Reg. 611 

Examination of test specimens for initial qualification tests:-

(a)
Groove welded plate specimens

The Groove welded plate specimens after welding may be lightly pressed cold to remove any distortion due to welding. The test specimen shall be similarly treated as required for the actual production weld.

After visual examination, the welded specimen shall be subjected to radiographic examination in the manner as provided in Regulation 265 (b), provided that this requirement may be waived when the welder is to be engaged on production work where radiographic examination is not required under these Regulations.

Thereafter test pieces shall be marked and cut out in order shown in Figure XIII/1.

The bend test specimens (B1 & B2) shall be prepared and tested as per Regulations 261 & 262. In the case of alloy steel specimen, the angle of the bend is to be decided by the Competent Authority, provided that the angle shall, in no case, be less than 120°.

Two each specimens (E1 & E2) shall be prepared, one for micro and the other for macro examination as per Regulations 265(a).

(b) Fillet welded plate specimens.-

The dimensions and preparation of the fillet-weld test specimen shall conform to Figure XIII/2. The test specimen shall not contain any visible cracks. It shall be cut transversely to provide a centre section (254 mm) (10 in.) long and two end sections each approximately (25 mm) (1 in.) long.

The stem of the (254 mm) (10 in.) centre section shall be loaded laterally in such a way that the root of the weld is in tension. The laod shall be steadily increased until the specimen fractures or bends flat upon itself. In order to pass the test.-


(1) The specimen shall not fracture, or
(2) If it fractures, the fractured surface shall show no evidence of cracks or incomplete root penetration, and the sum of the lengths of inclusions and gas pockets visible on the fractured surface shall not exceed (51 mm) (2 in.).

The cut end of one of the end sections shall be polished and etched with a suitable reagent to give a clear definition of the structure of the weld.
In order to pass the test:-
(i) Visual examination of the cross section of the weld shall show complete fusion at the root and freedom from cracks.
(ii) The weld shall not have a concavity or convexity greater than (1.6 mm.) (1/16 in.); and
(iii) There shall be not more than (1.6 mm) (1/16 in.) difference in the lengths of the legs of the fillet.
Earlier text: the 2008 DIPP web edition

(c), Reg. 611 (d), Reg. 611 (e)

QUALIFICATION TESTS FOR WELDERS ENGAGED IN WELDING OF BOILERS AND STEAM-PIPES UNDER CONSTRUCTION, ERECTION AND FABRICATION AT SITE IN INDIA AND IN REPAIRING BOILERS AND STEAM-PIPES BY WELDING

(c)Groove and fillet welded pipe and tube specimens

The groove welded pipe and tubes specimens shall be marked and test pieces cut out as in Figure XIII/3. The test pieces shall be prepared for face bend, root bend and etch test.

The pieces shall not be flattened, but tested in their curved conditions. The penetration bead may be removed to 0.8 mm. (1/32”) proud of the surface of the material.

Fillet welded branches shall be tested for:-

(i)Visual examination:-

The test welds so obtained shall be visually examined for root penetration, freedom from undercut, disposition of runs, uniformity of surface, shape of profile, smoothness of joint, freedom from cavities and slag, dimensions of weld deposit, quality of weld metal (overheating, surface cracks, spongy surface, etc.). Any piece showing serious defects shall be rejected.

(ii)Macro examination:-

Each branch weld test piece shall be sawn as shown in Figure XIII/4 and each portion so produced shall be prepared and etched. The sections shall then be examined for degree of fusion, degree of root penetration, absence of nonmetalic (slag) inclusions and quality of weld metal. The joint should show good root fusion, complete freedom from basal cracking, and the absence of any but very minor defects.

(d)Welded Tube Joints

A test length approximately 203 mm long shall be cut from the tube with the welded joint disposed approximately at the centre. After visual examination, one test piece not exceeding 13 mm. for tubes 6 mm in thickness and below and thrice the thickness of the tube for thickness of over 6 mm. shall be cut longitudinally. The test piece shall not be less than 76 mm. in length on either side of the weld. The slight excess of internal bead may be filed until it is not more than 0.8 mm. proud of the general surface. The test piece shall then be bent back with the root in tension through 90 degree round a former of diameter equal to three times the thickness of the tubes. With regard to alloy steel pipes and tubes, the bend test specimen shall be bent without being straightened, but after removal of the weld reinforcement down to the level of but not below the surface round a former of diameter 4t and through an angle of 90°. The bending may be carried out by blows or by pressure. Care shall be taken to ensure that the former is so positioned that the weld is maintained at the crown of the bend. The test specimen shall be capable of being bent through 90 degree without signs of failure, although slight premature failure at the edges of a specimen need not be considered a cause for rejection. The opening out of a slight defect due to incomplete root penetration or lack of root fusion need not be considered a cause for rejection, provided the defect has sound metal at the back and on

either side of it.

(e)Additional tests before rejection

Should any of the test pieces tested in accordance with the above sub-regulations fail to meet the specified requirements, one further strip may be cut from the specimen and subjected to the same test. If any test piece does not reach the required standard two further welds shall be made and the procedure in the above sub-regulation repeated. If any of these welds does not reach the required standard, the welder shall be deemed not to have qualified for a certificate.

Amendments found

Machine-assisted list from the amending notifications (DPIIT copies; 1990–1998 from scanned Gazette issues on India Code); may be incomplete.

DateNotificationPartActionWhat changed (summary)Web edition
1994-11-23G.S.R. 607 OCR of scan(a)SubstitutedChanges the word "X-Ray" to "radiographic".listed before the capture
2010-10-28G.S.R. 195(f), (g)InsertedInserts a right to be heard before refusal of a welder certificate and makes the decision final.listed before the capture