Indian Boiler Regulations, 1950 (superseded 1 Oct 2026)
Regulation 50 — Additional tests before rejection
Text in the DPIIT web edition
Archived copy captured 03 Aug 2022 (Wayback Machine). This page was revised after the 2019 capture, so later amendments may be included. Units as printed.
| [image] | [image] |
| ||||||||||||||||
Earlier text: the 2008 DIPP web edition
MATERIALS OF CONSTRUCTION
SEAMLESS MOLYBDENUM STEEL BOILER AND SUPERHEATER TUBES FOR DESIGN METAL TEMPERATURES NOT EXCEEDING 510 DEGREE C (950 DEGREE F).
Additional tests before rejection
Should a tube selected for testing purpose show definite signs of failure in any one or more of the tests specified in Regulations 49(a), 49(b) and 49(c), two further tests of the same kind may be made at the option of the manufacturer from two additional tubes selected from the same batch. If the repeat tests are satisfactory the tubes shall be accepted provided that in all other respects they fulfill the conditions of this standard. Should either of the tubes fail in any tests, the batch of tubes represented may be re-heat-treated in accordance with Regulation 48
(b)and then retested in accordance with Regulations 49(a), 49(b) and 49(c), but employing twice the number of test pieces. If these second repeat tests are satisfactory, the tubes shall be accepted provided that in all other respects they fulfill the conditions of this standard; but if definite defects are again shown, the batch of tubes which the test pieces represent shall be rejected.
Amendments found
Machine-assisted list from the amending notifications (DPIIT copies; 1990–1998 from scanned Gazette issues on India Code); may be incomplete.
| Date | Notification | Part | Action | What changed (summary) | Web edition |
|---|---|---|---|---|---|
| 2001-04-10 | G.S.R. 219 | Substituted | Replaced as part of the block substitution of regulations 36 to 56 (tube specifications). | listed before the capture |