Indian Boiler Regulations, 1950 (superseded 1 Oct 2026)
Regulation 265B — Radiographical Examination
Text in the DPIIT web edition
Archived copy captured 20 Nov 2019 (Wayback Machine); the same page also prints regulations 264, 265, 265A. The text matches the 2019 capture; amendments from 2020 onwards are probably not included. Units as printed.
|
| ||||||||||||||
Reg. 265 Non-Destructive Tests
Reg. 265 (b) Radiographical Examination
|
Earlier text: the 2008 DIPP web edition
Radiographical Examination
Every portion of the longitudinal and circumferential welded joints of the drums shall be subjected to radiographical examination or ultrasonic examination. Where ultrasonic examination is used, it shall be demonstrated to the satisfaction of the Inspecting Authority that the equipment and the technique used are satisfactory. The manufacturer shall ensure that the operator employed is competent to use the equipment, apply the technique and interpret the results of the examination.
The method employed in obtaining the radiographs shall be such as to show clearly defects having a magnitude equal to 2 per cent of the thickness of the welded joint. To determine whether this result is being obtained and indicator of approved form which includes a portion equivalent to not more than 2 per cent of the joint thickness, shall be placed in the vicinity of the weld so as to make a record on each radiograph.
Each section of every weld shall be marked so that the radiographs can be easily correlated to the particular part of the joint represented.
The examination shall be made from the original films and the acceptability of the welds shall be decided by the Inspecting Authority. The welds deemed unsatisfactory shall be rejected or dealt with under Regulation 266 and be radiographed again.