BETAIndependent engineering reference. Source-text verification is ongoing.Verification ongoing.Verification status →
IBRsourceIndian Boiler Regulations, made clear

Indian Boiler Regulations, 1950 (superseded 1 Oct 2026)

Regulation 392G

Unofficial DPIIT web edition · not verified0 amendments found

Text in the DPIIT web edition

Archived copy captured 03 Aug 2022 (Wayback Machine); the same page also prints regulations 392H, 392I, 392J. The text matches the 2019 capture; amendments from 2020 onwards are probably not included. Units as printed.

Unofficial DPIIT web edition · archived 2022 · not checked against the Gazette

Reg. 392 g, Reg. 392 h, Reg. 392 i, Reg. 392 j

(g) The thickness of a patch plate shall not be less than the original thickness of the plate which it is used to patch.


Reg. 392 h

Bulged or distorted furnaces of circular section may, if the bulge or distortion is not too great, be pressed back to shape.


Reg. 392 i

Circular furnaces of horizontal boilers that have become distorted may be suitably reinforced.


Reg. 392 j
Anti-collapse rings shall be of substantial section either of single or double angles bolted back to back with screw stays not less than 7/8th inch in diameter and about 7 inches in pitch passes through flat of angle and screwed into the Furnace, the ends being either rounded or riveted over on the fire side and fitted with nuts at the other. The stay bolts shall be fitted with ferrules not less than 1 inch in depth between furnace and angle ring.
Earlier text: the 2008 DIPP web edition

REGULATIONS FOR THE REGISTRATION OF BOILERS AND INSPECTION OF BOILERS AND STEAM-PIPES

The thickness of a patch plate shall not be less than the original thickness of the plate which it is used to patch.