Indian Boiler Regulations, 1950 (superseded 1 Oct 2026)
Regulation 390I — Tubes -Their defects, etc
Text in the DPIIT web edition
Archived copy captured 03 Aug 2022 (Wayback Machine); the same page also prints regulations 390G, 390H. The text matches the 2019 capture; amendments from 2020 onwards are probably not included. Units as printed.
| Reg. 390 g
Reg. 390 h
Reg. 390 i
|
Earlier text: the 2008 DIPP web edition
Tubes -Their defects, etc
(i)Tubes in horizontal fire-tube boilers deteriorate more rapidly at the ends toward the fire, and they should be carefully tapped with a light hammer on their outer surface to ascertain whether there has been serious reduction in thickness. The tubes of vertical tubular boilers are more susceptible to deterioration at the upper ends open when exposed to the products of combustion without water protection. They should be reached as far as possible either through the handholes, if any, or inspected at the ends.
(ii)The surfaces should be carefully examined to detect bulges or cracks, or any evidences or defective welds. Where there is a strong draft, the tubes may become thinned by corrosion produced by the impingement of particles of fuel and ash, or the improper use of soot blowers. A leak from a tube frequently causes serious corrosive action on a number of tubes in its immediate vicinity.
(iii)Where short tubes or nipples are employed in joining drums or headers, there is a tendency for waste products of the furnace to lodge in the junction points and such deposits are likely to cause corrosion if moisture is present. All such places should be thoroughly cleaned and examined.