BETAIndependent engineering reference. Source-text verification is ongoing.Verification ongoing.Verification status →
IBRsourceIndian Boiler Regulations, made clear

Indian Boiler Regulations, 1950 (superseded 1 Oct 2026)

Regulation 39 — Flattening Test

Unofficial DPIIT web edition · not verified3 amendments found

Text in the DPIIT web edition

Archived copy captured 03 Aug 2022 (Wayback Machine). The text matches the 2019 capture; amendments from 2020 onwards are probably not included. Units as printed.

Unofficial DPIIT web edition · archived 2022 · not checked against the Gazette
Reg. 39
MATERIALS OF CONSTRUCTION

COLD DRAWN SEAMLESS CAR BON STEEL BOILER, SUPERHEATER AND HEAT EXCHANGER TUBES FOR DESIGN METAL TEMPERATURES NOT EXCEEDING 454°C (850°F).

Flattening Test

A section of the tube not less than 63 mm in length shall be flattened cold between two parallel flat surfaces to a distance between the plates (H) as calculated by the formula given below, without showing any sign of a crack or flaw.
            (1 + e) t
H =  -----------------
            E + t/D

where t   = specified thickness of tube (mm)

           D = specified outside diameter of the tube (mm)

                       e  = a constant, as given below

e = 0.07 for Carbon steel with maximum specified carbon 0.19% or greater

e = 0.09 for Carbon steel with  maximum specified carbon 0.18% or less

Earlier text: the 2008 DIPP web edition

MATERIALS OF CONSTRUCTION

COLD DRAWN SEAMLESS STEEL BOILER AND SUPERHEATER TUBES FOR DESIGN METAL TEMPERATURES NOT EXCEEDING 454°C (850°F).

Flattening Test

A ring not less than 50 mm in length cut from one end of each selected tube shall be flattened between two parallel flat surfaces to a distance between the plates (H) as calculated by the formula given below without showing any sign of a crack or flaw:

   (1+C)a
H=---------
   a
   C+ ----
   D

where a = thickness of tube (mm)

D = outside diameter of the tube (mm)

C = a constant as given below

C = 0.09 for steel having a specified minimum tensile strength from 31 kgf/mm2 upto and including 35 kgf/mm2.

C = 0.07 for steel having a specified minimum tensile strength over 35 kgf/mm2 upto and including 42 kgf/mm2

C = 0.05 for steel having a specified minimum tensile strength over 42 kgf/mm2 upto and including 50 kgf/mm2.

C = 0.03 for steel having a specified minimum tensile strength over 50 kgf/mm2 upto and including 62 kgf/mm2.

Amendments found

Machine-assisted list from the amending notifications (DPIIT copies; 1990–1998 from scanned Gazette issues on India Code); may be incomplete.

DateNotificationPartActionWhat changed (summary)Web edition
1969-03-01/1988-12-31compilation-1969-1988#p17 OCR of compilationSubstitutedReplaces regulation 39 (flattening test).listed before the capture
2001-04-10G.S.R. 219SubstitutedReplaced as part of the block substitution of regulations 36 to 56 (tube specifications).listed before the capture
2007-03-12G.S.R. 46 (copy) 2008 web editionSubstitutedSubstitutes the flattening test: flatten to H = (1+e)t/(e+t/D), with e = 0.07 or 0.09 by carbon content; two-step ductility and soundness test.
Uncertain: Text from the unofficial 2008 DIPP web edition; G.S.R. number as published unconfirmed.
listed before the capture