Indian Boiler Regulations, 1950 (superseded 1 Oct 2026)
Regulation 36 — Material process
Text in the DPIIT web edition
Archived copy captured 03 Aug 2022 (Wayback Machine). The text matches the 2019 capture; amendments from 2020 onwards are probably not included. Units as printed.
| Reg. 36 MATERIALS OF CONSTRUCTION COLD DRAWN SEAMLESS CARBON STEEL BOILER, SUPERHEATER AND HEAT EXCHANGER TUBES FOR DESIGN METAL TEMPERATURES NOT EXCEEDING 454°C (850°F). |
| 36.(a) General.- (i) These regulations cover both hot finished and cold drawn seamless boiler, superheater and heat exchanger tubes, which shall conform in all respects with the requirements herein specified. (ii)The seamless tubes conforming to other national or international standards which are known to be commonly used as being suitable for use as boiler, superheater and heat exchanger tubes can also be used with the designations of the national or international standards, provided such materials are not specifically prohibited by the regulations. (iii) While making tubes to other national/international standards the allowable stresses of the respective standards shall be strictly followed while designing the tubes. (b) Material. - (i)The tubes shall be seamless and manufactured from steel produced by an open hearth or electric process or any of the oxygen processes. The steel shall be fully killed. (ii)The steel shall conform to the following limits of chemical composition. Chemical composition (%)
* For grade TB and TC for each reduction of 0.01% below the specified carbon maximum, an increase of 0.06% Manganese above the specified maximum will be permitted up to a maximum of 1.35%. (c) Heat Treatment.- Hot finished tubes need not be heat treated, cold drawn tubes shall be given a sub-critical annealing, a full anneal, or a normalising heat treatment after the final cold finishing process. (d) Workmanship and Tolerance.-The tubes shall be well finished, cleaned free from harmful defects. They shall be reasonably straight, smooth, cylindrical and subject to the following tolerances. Finished tubes shall be reasonably straight and have smooth ends free of burrs. They shall have a workmanlike finish. Surface imperfections like any discontinuity or irregularity found in the tube may be removed by grinding, provided that smooth curved surface is maintained, and the wall thickness is not decreased to less than that permitted. The outside diameter at the point of grinding may be reduced by the amount so removed. (i) Permissible variations in outside diameter.
(ii) Permissible variation in Wall Thickness in percentage.
(iii) Permissible variations in length
Note.- These permissible variations in lengths apply to cut lengths up to and including 7.3 m. For lengths over 7.3 m, an additional over tolerance of 3 mm for each 3 m or fraction thereof, shall be permissible, up to a maximum of 13 mm. Length tolerances on the positive side other than specified may be mutually agreed. | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
Earlier text: the 2008 DIPP web edition
MATERIALS OF CONSTRUCTION
COLD DRAWN SEAMLESS STEEL BOILER AND SUPERHEATER TUBES FOR DESIGN METAL TEMPERATURES NOT EXCEEDING 454°C (850°F).
(a)Material process - The tubes shall be seamless and made of steel produced by an Open Hearth or Electric process or any of the oxygen processes. The steel shall not contain more than 0.05 per cent of sulphur or phosphorus. The manufacturers shall supply a certificate of analysis when required to do so.
(b)Annealing - The tubes shall be carefully annealed throughout their length after the operation of drawing and the ends shall be carefully annealed after the process of swelling or reducing the diameter.
(c)Freedom from Defects - The tubes both internally and externally shall be sound, clean, smooth, well finished and free from surface defects, rust, longitudinal seaming and grooving. The ends shall be clean and square.
(d)Tolerances -
(i)Thickness.- The tolerance in thickness shall be 5 per cent below and 10 per cent above the specified thickness.
(ii)Swelled or Reduced Ends.- Where the ends of tubes are swelled or reduced the thickness at the ends may be reduced, or increased under or over, the actual thickness of the tubes by an amount strictly in proportion to the percentage of such swelling or reducing and in addition to this allowance the tolerances specified in paragraph (i) of this sub-regulation shall also apply.
(iii)Diameter.- The external diameter of the tubes, measured at any point shall be not greater than the specified, but may be less by not more than 1 per cent.
(iv)Length.- The length of the tubes shall be not less than the nominal length but may exceed it by the amount given below:-
Upto and including 30 ft…………………... 1/2 inch
Over 30 ft………………………………… 1/4 inch
NOTE.- Where the materials used for designed temperature above 750°F (399°C) the steel shall be of non-segregated or fully killed type.
Amendments found
Machine-assisted list from the amending notifications (DPIIT copies; 1990–1998 from scanned Gazette issues on India Code); may be incomplete.
| Date | Notification | Part | Action | What changed (summary) | Web edition |
|---|---|---|---|---|---|
| 2001-04-10 | G.S.R. 219 | Substituted | Replaced as part of the block substitution of regulations 36 to 56 (tube specifications). | listed before the capture | |
| 2004-08-02 | G.S.R. 265 | (b)(ii), (d) | Amended | Corrects the sulphur limit for Grade TC (0.35 to 0.035) and replaces two chart entries with 'NA'. | listed before the capture |