Indian Boiler Regulations, 1950 (superseded 1 Oct 2026)
Regulation 347C — Reg. 347 D, Reg. 347 E
Text in the DPIIT web edition
Archived copy captured 03 Aug 2022 (Wayback Machine); the same page also prints regulations 347D, 347E. The text matches the 2019 capture; amendments from 2020 onwards are probably not included. Units as printed.
| Reg. 347 C Reg. 347 D, Reg. 347 E
|
Earlier text: the 2008 DIPP web edition
Reg. 347 D, Reg. 347 E
Bend test on the weld
A strip not less than 38mm. (1-1/2 in.) Wide cut circumferentially from one end of each selected pipe with the weld near the middle of the strip, shall when cold withstand, without showing either crack or flaw, being doubled over in the direction of original curvature round a bar, the diameter of the bar being equal to eight times the thickness of the test piece, the weld being placed at the point of maximum bending.
In cases where the outside diameter of the pipe is less than 8 times the wall thickness, the diameter of the former shall be equal to 4t or 2/3rd of the nominal bore of the pipe, whichever is less.