BETAIndependent engineering reference. Source-text verification is ongoing.Verification ongoing.Verification status →
IBRsourceIndian Boiler Regulations, made clear

Indian Boiler Regulations, 1950 (superseded 1 Oct 2026)

Regulation 15 — Tensile Test pieces

Unofficial DPIIT web edition · not verified0 amendments found

Text in the DPIIT web edition

Archived copy captured 03 Aug 2022 (Wayback Machine). The text matches the 2019 capture; amendments from 2020 onwards are probably not included. Units as printed.

Unofficial DPIIT web edition · archived 2022 · not checked against the Gazette
Reg. 15
MATERIALS OF CONSTRUCTION

STEEL PLATES, RIVETS, SECTION AND BARS IN CARBON STEEL

Tensile Test pieces

(a) The tensile strength and percentage elongation shall be determined from test pieces of gauge lengths preferably equal to Lo=5.6(Ao)1/2 (see regulation 16). Alternatively, other gauge lengths may be used, provided the elongation is expressed as the equivalent value on a gauge length of 5.65(Ao)1/2.

(b) In arbitration cases, a test piece of gauge length equal to 5.65(Ao)1/2 for rectangular test piece or 5 do for round test pieces shall be used. For plate thickness exceeding 60mm, test pieces shall be taken from the exterior third of the plate cross section. Wherever practicable, the rolled surface shall be retained on two opposite sides of the test piece.

Earlier text: the 2008 DIPP web edition

MATERIALS OF CONSTRUCTION

STEEL PLATES, RIVETS, SECTION AND BARS IN CARBON STEEL

Tensile Test pieces

(a)The tensile strength and percentage elongation shall be determined from test pieces of gauge lengths preferably equal to Lo=5.6(Ao)¹ᐟ² (see regulation 16). Alternatively, other gauge lengths may be used, provided the elongation is expressed as the equivalent value on a gauge length of 5.65(Ao)¹ᐟ².

(b)In arbitration cases, a test piece of gauge length equal to 5.65(Ao)¹ᐟ² for rectangular test piece or 5 do for round test pieces shall be used. For plate thickness exceeding 60mm, test pieces shall be taken from the exterior third of the plate cross section. Wherever practicable, the rolled surface shall be retained on two opposite sides of the test piece.