Indian Boiler Regulations, 1950 (superseded 1 Oct 2026)
Regulation 99 — Preparation of Plates
Text in the DPIIT web edition
Archived copy captured 03 Aug 2022 (Wayback Machine); the same page also prints regulations 100, 101. The text matches the 2019 capture; amendments from 2020 onwards are probably not included. Units as printed.
| Reg. 99, Reg. 100, Reg. 101 CONSTRUCTION AND WORKMANSHIP GENERAL |
| The edges of all plates and butt straps shall be machined or flame-cut by machine and the caulking edges shall be beveled to an angle not sharper than 70 degrees to the plane of the plate and between 70 and 80 degrees wherever practicable. GENERAL All steel plates which are dished, flanged or locally heated shall be afterwards normalized unless they have been heated during the operation within the normalizing range. Reg. 101 GENERAL No boiler plate shall be less than ¼ inch in thickness. |
Earlier text: the 2008 DIPP web edition
CONSTRUCTION AND WORKMANSHIP
GENERAL
Preparation of Plates
The edges of all plates and butt straps shall be machined or flame-cut by machine and the caulking edges shall be beveled to an angle not sharper than 70 degrees to the plane of the plate and between 70 and 80 degrees wherever practicable.
Plates which are to be flame-cut by machine without heat treatment or subsequent grinding or machining shall not have a carbon content higher than 0.26 per cent.
Where the carbon content exceeds 0.26 per cent heat treatment, grinding or machining shall be carried out.
The edges of all plates shall have a smooth finish.