Regulation 9 — Process of manufacture

Unofficial DPIIT web edition · not verified1 amendment found

Text in the DPIIT web edition

Archived copy captured 03 Aug 2022 (Wayback Machine). The text matches the 2019 capture; amendments from 2020 onwards are probably not included. Units as printed.

Unofficial DPIIT web edition · archived 2022 · not checked against the Gazette
Reg. 9
MATERIALS OF CONSTRUCTION

STEEL PLATES, RIVETS, SECTION AND BARS IN CARBON STEEL

Process of manufacture

(a) Steel for plates shall be made by the open hearth, electric furnace or basic oxygen process or any other process which gives steel having equivalent specified properties.

(b) General deoxidation practice shall be appropriate to the type of steel used, particularly where the deoxidation practice influences the level of the elevated temperature properties of steel.

(c) Rimmed steels may be permitted only for riveted drums or shells made of plates having a nominal thickness upto 20 mm.

(d) Plates of carbon steel shall conform to one of the following four grades of tensile strength:-

(i) 37 to 45 kgf/mm2
(ii) 42 to 50 kgf/mm2
(iii) 47 to 56 kgf/mm2
(iv) 52 to 62 kgf/mm2

(e) Semi-killed steel may be used for plates in C and C-Mn steel with an upper limit of the tensile strength not exceeding 56 kg /mm2 and with thickness not exceeding 50mm under service temperature condition 0-450°C.


Earlier text: the 2008 DIPP web edition

MATERIALS OF CONSTRUCTION

STEEL PLATES, RIVETS, SECTION AND BARS IN CARBON STEEL

Process of manufacture

(a)Steel for plates shall be made by the open hearth, electric furnace or basic oxygen process or any other process which gives steel having equivalent specified properties.

(b)General deoxidation practice shall be appropriate to the type of steel used, particularly where the deoxidation practice influences the level of the elevated temperature properties of steel.

(c)Rimmed steels may be permitted only for riveted drums or shells made of plates having a nominal thickness upto 20 mm.

(d)Plates of carbon steel shall conform to one of the following four grades of tensile strength:-

(i)37 to 45 kgf/mm2

(ii)42 to 50 kgf/mm2

(iii)47 to 56 kgf/mm2

(iv)52 to 62 kgf/mm2

(e)Semi-killed steel may be used for plates in C and C-Mn steel with an upper limit of the tensile strength not exceeding 56 kg /mm2 and with thickness not exceeding 50mm under service temperature condition 0-450°C.

Amendments found

Machine-assisted list from the amending notifications (DPIIT copies; 1990–1998 from scanned Gazette issues on India Code); may be incomplete.

DateNotificationPartActionWhat changed (summary)Web edition
1969-03-01/1988-12-31compilation-1969-1988#p11 OCR of compilationSubstitutedReplaces regulation 9 (process of manufacture of steel for plates).listed before the capture