Indian Boiler Regulations, 1950 (superseded 1 Oct 2026)
Regulation 49B — Flattering Test
Text in the DPIIT web edition
Archived copy captured 03 Aug 2022 (Wayback Machine). The text matches the 2019 capture; amendments from 2020 onwards are probably not included. Units as printed.
| Reg. 49 B MATERIALS OF CONSTRUCTION SEAMLESS FERRITIC AND AUSTENITIC ALLOY STEEL BOILER, SUPERHEATER AND HEAT EXCHANGER TUBES |
| A section of the tube not less than 63 mm in length shall be flattened cold between two parallel flat surfaces to a distance between the plates (H) as calculated by the formula given below, without showing any sign of a crack of flaw. (1 + e)t
H = -----------
e + t/D where t = specified thickness of tube (mm) D = specified outside diameter of the tube (mm) e = a constant, as given below e = 0.08 for ferritic alloy steel e = 0.09 for austenitic steel |
Earlier text: the 2008 DIPP web edition
MATERIALS OF CONSTRUCTION
SEAMLESS MOLYBDENUM STEEL BOILER AND SUPERHEATER TUBES FOR DESIGN METAL TEMPERATURE NOT EXCEEDING 510 DEGREE C (950 DEGREE F).
Flattening Test
A ring not less than 2 inches in length cut from one end of each selected tube shall be flattened between two parallel flat surfaces the width of which shall be not less than 1½ times the diameter of the tube. Where the pressure is released, the interior surfaces of the test piece (at the middle) shall remain at a distance apart of not more than three times the specified thickness of the tube and the test piece shall then show no sign of crack of flaw.
The flattening test carried out in accordance with any other standard Code may be accepted in which case the Code adopted shall be specified.