BETAIndependent engineering reference. Source-text verification is ongoing.Verification ongoing.Verification status →
IBRsourceIndian Boiler Regulations, made clear

Indian Boiler Regulations, 1950 (superseded 1 Oct 2026)

Regulation 392K

Unofficial DPIIT web edition · not verified0 amendments found

Text in the DPIIT web edition

Archived copy captured 03 Aug 2022 (Wayback Machine); the same page also prints regulations 392L, 392M. The text matches the 2019 capture; amendments from 2020 onwards are probably not included. Units as printed.

Unofficial DPIIT web edition · archived 2022 · not checked against the Gazette

Reg. 392 k, Reg. 392 l, Reg. 392 m

(k) Welding shall not be accepted for the repair of any part of a boiler for which welding is forbidden for a new boiler under these Regulations. Boiler shells shall not be repaired by welding beyond the filling up of a small isolated corroded or pitted part or the making up of wasted edges of openings.


Reg. 392 l

Cracks or grooving in dished or flat end plates of cylindrical shells or in the bends of furnace flanges in a circumferential direction may be weed out and welded.


Reg. 392 m
Wasted parts of circular furnaces and fire-boxes and fire exposed flat plates as in rectangular fire-boxes and combustion chambers may be cut out and be replaced by new pieces welded in or they may be built up by welding. Longitudinal cracks in circular furnaces and fire-boxes and cracks in rectangular fire-boxes and combustion chambers may be welded.
Earlier text: the 2008 DIPP web edition

REGULATIONS FOR THE REGISTRATION OF BOILERS AND INSPECTION OF BOILERS AND STEAM-PIPES

Welding shall not be accepted for the repair of any part of a boiler for which welding is forbidden for a new boiler under these Regulations. Boiler shells shall not be repaired by welding beyond the filling up of a small isolated corroded or pitted part or the making up of wasted edges of openings.