BETAIndependent engineering reference. Source-text verification is ongoing.Verification ongoing.Verification status →
IBRsourceIndian Boiler Regulations, made clear

Indian Boiler Regulations, 1950 (superseded 1 Oct 2026)

Regulation 266E — Examination before Re-welding

Unofficial DPIIT web edition · not verified0 amendments found

Text in the DPIIT web edition

Archived copy captured 03 Aug 2022 (Wayback Machine); the same page also prints regulations 266D, 266F, 266G, 266H, 266I. The text matches the 2019 capture; amendments from 2020 onwards are probably not included. Units as printed.

Unofficial DPIIT web edition · archived 2022 · not checked against the Gazette


Reg. 266 d, Reg. 266 e, Reg. 266 f, Reg. 266 g, Reg. 266 h,
Reg. 266 i

Removal of Defects
Defects shall be cut out by chipping or machining or by burning out by the "Air Arc Weld Process”.


Reg. 266 e

Examination before Re-welding

Where a defective part has been cut out, the Inspecting Authority shall be entitled to make an examination before re-welding.



Reg. 266 f

Process used for Repairs

Only metallic arc welding shall be used for repairs.



Reg. 266 g

Radiographical Examination after Repairs

All repaired areas shall be subjected to radiographic or radioscopic examination by the approved techniques.



Reg. 266 h

Specimen Representing Repairs

The Inspecting Authority shall be entitled to call for specimens representing any welded repair, for the purpose of examination and test.



Reg. 266 i

Diagram of Welded Repairs

On completion of all welded repairs the manufacturers shall, if requested, supply for record purposes a detailed diagram showing the position, length, depth and width of all such repairs.

Earlier text: the 2008 DIPP web edition

Examination before Re-welding

Where a defective part has been cut out, the Inspecting Authority shall be entitled to make an examination before re-welding.