Indian Boiler Regulations, 1950 (superseded 1 Oct 2026)
Regulation 252 — Method of making welded joints
Text in the DPIIT web edition
Archived copy captured 03 Aug 2022 (Wayback Machine); the same page also prints regulations 250, 251, 253. The text matches the 2019 capture; amendments from 2020 onwards are probably not included. Units as printed.
|
| |||||
Reg.251 Cylindrical shells of drums
Reg.252 Method of making welded joints
Reg.253
| |||||
Earlier text: the 2008 DIPP web edition
Method of making welded joints
Provided the requisite quality of welding is achieved, the seams may be welded from both sides of the plate or from one side of the plate with or without a backing strip. If a backing strip is used, it shall be removed and the surface so exposed shall be dressed.
Additional runs of metal shall be deposited at the surface of the welded seams so that the welded metal at the level of the surfaces of the plate is refined as far as possible. The surfaces of the weld shall thereafter be machined or ground so as to provide smooth contours and to be flush with the respective surfaces of the plate. There shall be no undercutting at the junctions.
When affixing standpipes, branch pipes, seatings, compensating plates, doubling plates or manhole frames, not less than two runs of metal shall be deposited at each weld. Each run of weld shall be thoroughly cleaned and freed from slag that may adversely affect the quality of the succeeding runs. Welds shall be marked permanently to facilitate their location.