BETAIndependent engineering reference. Source-text verification is ongoing.Verification ongoing.Verification status →
IBRsourceIndian Boiler Regulations, made clear

Indian Boiler Regulations, 1950 (superseded 1 Oct 2026)

Regulation 24 — Defacing of rejected material

Unofficial DPIIT web edition · not verified1 amendment found

Text in the DPIIT web edition

Archived copy captured 03 Aug 2022 (Wayback Machine). The text matches the 2019 capture; amendments from 2020 onwards are probably not included. Units as printed.

Unofficial DPIIT web edition · archived 2022 · not checked against the Gazette
Reg. 24
MATERIALS OF CONSTRUCTION

STEEL PLATES, RIVETS, SECTION AND BARS IN CARBON STEEL

Defacing of rejected material

In the event of the material failing in any case to withstand the prescribed tests, the identification mark of the Inspecting officer which has been stamped on the material, shall be defaced by punch marks extending beyond the identification mark, in the form of a cross, thus denoting that the material has failed.
Earlier text: the 2008 DIPP web edition

MATERIALS OF CONSTRUCTION

STEEL PLATES, RIVETS, SECTION AND BARS IN CARBON STEEL

Defacing of rejected material

In the event of the material failing in any case to withstand the prescribed tests, the identification mark of the Inspecting officer which has been stamped on the material, shall be defaced by punch marks extending beyond the identification mark, in the form of a cross, thus denoting that the material has failed.

Amendments found

Machine-assisted list from the amending notifications (DPIIT copies; 1990–1998 from scanned Gazette issues on India Code); may be incomplete.

DateNotificationPartActionWhat changed (summary)Web edition
2010-10-07G.S.R. 821(E)AmendedReplaces 'Inspecting officer(s)' with 'Competent Person' wherever it occurs.listed before the capture