BETAIndependent engineering reference. Source-text verification is ongoing.Verification ongoing.Verification status →
IBRsourceIndian Boiler Regulations, made clear

Indian Boiler Regulations, 1950 (superseded 1 Oct 2026)

Regulation 22 — Additional tests before rejection

Unofficial DPIIT web edition · not verified1 amendment found

Text in the DPIIT web edition

Archived copy captured 03 Aug 2022 (Wayback Machine). The text matches the 2019 capture; amendments from 2020 onwards are probably not included. Units as printed.

Unofficial DPIIT web edition · archived 2022 · not checked against the Gazette
Reg. 22
MATERIALS OF CONSTRUCTION

STEEL PLATES, RIVETS, SECTION AND BARS IN CARBON STEEL

Additional tests before rejection

Should the test pieces first selected by the Inspector or Inspecting Officer not fulfil the test requirements, two further tests of the same kind may be made, but should either of these fail, the plates or bars from which test pieces were cut shall be rejected. In all such cases further tests shall be made before any material from the same charge can be accepted.

If the unsatisfactory result of a test is obviously due to technical conditions of the testing method or to a closely limited defects of a test piece, then the failure can be left out of consideration in the decision on the fulfilment of the requirement and another test piece may be substituted. If the unsatisfactory result of test is due to an unfavourable heat treatment the plate and the test strip may be heat treated again. Following this, the entire test shall be repeated.

Earlier text: the 2008 DIPP web edition

MATERIALS OF CONSTRUCTION

STEEL PLATES, RIVETS, SECTION AND BARS IN CARBON STEEL

Additional tests before rejection

Should the test pieces first selected by the Inspector or Inspecting Officer not fulfil the test requirements, two further tests of the same kind may be made, but should either of these fail, the plates or bars from which test pieces were cut shall be rejected. In all such cases further tests shall be made before any material from the same charge can be accepted.

If the unsatisfactory result of a test is obviously due to technical conditions of the testing method or to a closely limited defects of a test piece, then the failure can be left out of consideration in the decision on the fulfilment of the requirement and another test piece may be substituted. If the unsatisfactory result of test is due to an unfavourable heat treatment the plate and the test strip may be heat treated again. Following this, the entire test shall be repeated.

Amendments found

Machine-assisted list from the amending notifications (DPIIT copies; 1990–1998 from scanned Gazette issues on India Code); may be incomplete.

DateNotificationPartActionWhat changed (summary)Web edition
2010-10-07G.S.R. 821(E)AmendedReplaces 'Inspector or Inspecting officer' with 'Competent Person'.listed before the capture