Indian Boiler Regulations, 1950 (superseded 1 Oct 2026)
Regulation 185 — Circumferential and End Seams of Water Tube Boilers
Text in the DPIIT web edition
Archived copy captured 03 Aug 2022 (Wayback Machine). The text matches the 2019 capture; amendments from 2020 onwards are probably not included. Units as printed.
| Reg. 185 SHELLS Circumferential and End Seams of Water Tube Boilers The suitability of circumferential seams including the seams joining ends to shells shall be verified by the following formula : -
Where K = 150 for 26/30 tons tensile plates. K = 157 for 28/32 tons tensile plates. Due to higher stresses, see regulations 271 and 340. WP = The working pressure in lbs per sq. in. D = The diameter of shell in inches, measured inside the outer ring of plates. J = Circumferential Joint efficiency calculated by Eqn.2 or 3. C = 8.24 where the seams are made with lap joints and are treble riveted. = 8.44 where the seams are made with lap joints and are double riveted. = 9.60 where the seams are made with lap joints and are single riveted. t = thickness of plate in 32nd of an inch. |
Earlier text: the 2008 DIPP web edition
SHELLS
Circumferential and End Seams of Water Tube Boilers
The suitability of circumferential seams including the seams joining ends to shells shall be verified by the following formula : -
K x J x (t-2)
is equal to or greater than W.P. Eqn. (17)
D x C
Where
K = 150 for 26/30 tons tensile plates.
K = 157 for 28/32 tons tensile plates.
Due to higher stresses, see regulations 271 and 340.
WP = The working pressure in lbs per sq. in.
D = The diameter of shell in inches, measured inside the outer ring of plates.
J = Circumferential Joint efficiency calculated by Eqn.2 or 3.
C = 8.24 where the seams are made with lap joints and are treble riveted.
= 8.44 where the seams are made with lap joints and are double riveted.
= 9.60 where the seams are made with lap joints and are single riveted.
t = thickness of plate in 32nd of an inch.