BETAIndependent engineering reference. Source-text verification is ongoing.Verification ongoing.Verification status →
IBRsourceIndian Boiler Regulations, made clear

Indian Boiler Regulations, 1950 (superseded 1 Oct 2026)

Regulation 125 — Fusion Welded Longitudinal Seams

Unofficial DPIIT web edition · not verified0 amendments found

Text in the DPIIT web edition

Archived copy captured 03 Aug 2022 (Wayback Machine). The text matches the 2019 capture; amendments from 2020 onwards are probably not included. Units as printed.

Unofficial DPIIT web edition · archived 2022 · not checked against the Gazette
Reg. 125
FURNACES
Fusion Welded Longitudinal Seams

Where the longitudinal seam is fusion welded the following precautions shall be observed :-

a) Plates 5/8 inch and above in thickness shall be bevelled from both sides of each abutting edge but the bevel need not necessarily be the same on each side (see Figs. 1 and 2). Plates, less than 5/8 inch in thickness may be beveled from one side only of each abutting edge (see Figs. 3 and 4).

The included angle of the bevel shall be not less than 60° and the beveling may be any one of the forms shown in Figs.1-4
b) In order to obtain full penetration of the weld metal a gap shall be maintained between the plates when they are being welded. Joints shall be welded from both sides, and the slag shall be removed after making each run. Before the second side of the joint is welded any slag or defect at the bottom of the first run shall be removed by grinding, chipping or machining. There shall be no appreciable undercutting of the plate.
c) For the purpose of relieving internal stresses the plates adjacent to a fusion weld shall be efficiently annealed after welding, and when the firebox is forge-welded it should be allowed to cool gradually.
Earlier text: the 2008 DIPP web edition

FURNACES

GENERAL

Fusion Welded Longitudinal Seams

Where the longitudinal seam is fusion welded the following precautions shall be observed :-

a)Plates 5/8 inch and above in thickness shall be bevelled from both sides of each abutting edge but the bevel need not necessarily be the same on each side (see Figs. 1 and 2). Plates, less than 5/8 inch in thickness may be beveled from one side only of each abutting edge (see Figs. 3 and 4).

The included angle of the bevel shall be not less than 60° and the beveling may be any one of the forms shown in Figs.1-4

b)In order to obtain full penetration of the weld metal a gap shall be maintained between the plates when they are being welded. Joints shall be welded from both sides, and the slag shall be removed after making each run. Before the second side of the joint is welded any slag or defect at the bottom of the first run shall be removed by grinding, chipping or machining. There shall be no appreciable undercutting of the plate.

c)For the purpose of relieving internal stresses the plates adjacent to a fusion weld shall be efficiently annealed after welding, and when the firebox is forge-welded it should be allowed to cool gradually.